Loading...

AZS

Material Alumina (Al2O3) - Zirconia (ZrO2) - Silica (SiO2)
Chemical Composition Al2O3: 40-50%, ZrO2: 32-41%, SiO2: 12-16%
Density 3.75 - 3.90 g/cm^3
Thermal Conductivity 3.2 - 3.6 W/m*K
Thermal Expansion 8 - 9 x 10^-6 /°C
Refractoriness (°C) 1750 - 1900°C
Crushing Strength 100 - 150 MPa
Application Glass melting furnaces, steelmaking furnaces, and
other high-temperature industrial applications.